- Maximum temperature 1730°C
- Maximum heating rate 65°C/minute
- Cycle time: from one to several hours depending on the zirconia
- 4 heating elements (rods) in MoSi2 (Molybdenum Disilicide)
- 3 trays for sinterizing with cover and zirconia pearls (capacity up to 50 units)
- Graphical cycles visualization
- Sintering single units in just one hour.
830 x 420 x 600 mm | 74 kg |